Details:

Molecular sieve 4A is made by raw powder, which has zeolite A crystal structure, with selected mineral binder. 4A Molecular sieve has an effective pore opening of 4Å (0.4nm), so molecules which diameter less than 4Å can be adsorbed. Mostly used for dehydration of natural gas.

Property unit Bead Pellet Note
8x12 4x8 1/16" 1/8"
Static Water Adsorption %wt ≥ 21.50 ≥ 21.50 ≥ 21.50 ≥ 21.50 RH50%, 25℃
Crush Strength N ≥ 30.00 ≥ 80.00 ≥ 30.00 ≥ 70.00 Avg. 25 beads
Crush Strength lbs ≥ 7.00 ≥ 18.00 ≥ 7.00 ≥ 16.00 Avg. 25 beads
Bulk Density g/ml ≥ 0.70 ≥ 0.70 ≥ 0.65 ≥ 0.65 Settled
Bulk Density  lbs/ft3 ≥ 43.00 ≥ 43.00 ≥ 40.00 ≥ 40.00 Settled
Loss on Ignition %wt ≤ 1.50 ≤ 1.50 ≤ 1.50 ≤ 1.50 575℃, 1hr
Loss on Attrition %wt ≤ 0.10 ≤ 0.10 ≤ 0.30 ≤ 0.30 ~
Particle Ratio % ≥ 97.00 ≥ 99.00 ~ ~ ~

Recommended Applications:
1. Drying of unsaturated hydrocarbons (e.g., ethylene, propylene, butadiene) 
2. Cracked Gas Drying.
3. Drying of natural gas.
4. Drying of highly polar compounds, such as methanol and ethanol. 