Raw material source
Properties
Price($/5g)
Bagasse
Microwave-Alkali extraction, Molecular weight 8000-20000g∕mol, Ash ≤0.06%, Lignin ≤0.8%
190
Bamboo
Microwave-Alkali extraction, Molecular weight 10000-20000g∕mol, Ash ≤0.05%, Lignin ≤0.8%
240
Eucalyptus
Alkali extraction, Molecular weight 9000-20000g∕mol, Ash ≤0.05%, Lignin ≤0.8%
250
Pine
Alkali extraction, Molecular weight 10000-20000g∕mol, Ash ≤0.04%, Lignin ≤0.7%
280
Questions or Bulk quote? All Celluloses